Steel No. |
COMPARABLE STANDARD |
(% ) CHEMICAL COMPOSITIONS |
||||||||||
AISI | JIS | DIN | C | Si | Mn | P | S | Ni | Cr | Mo | Cu | |
SCM440 | 4140 | SCM440 | 1.7225 | 0.38 - 0.43 | 0.15 - 0.35 | 0.60 - 0.85 | < 0.03 | < 0.03 | Max.0.25 | 0.90 - 1.20 | 0.15 - 0.30 | Max.0.30 |
2.MECHANICAL PROPERTY
eel No. |
SUPPLIED CONDITION |
YIELD STRENGTH, Kgf/mm2 |
TENSILE STRENGTH, Kgf/mm2 |
ELONGATION, % |
Reduction of Area, % |
Impact Energy, kgf/mm2 |
SCM440 | Forged & Normalized, Hardness 170-230 HB |
85 min. | 100 min | 12 min. | 45 min. | 6 min. |
3.APPLICATIONS
SCM440 is used for engineering structural, like high tensile shafts, bolts and nuts, gears, pinions and spindles. Locomotive traction with the big gear, supercharger drive gear, pressure vessel, rear axle, gear load of connecting rod and a spring clip,4140 can also be used to under 2000 m deep well of oil drill pipe joint and the fishing tool, and can be used for bending machine mould, etc
4.SUPPLY SIZE RANGE
Hot Rolled 4140 steel bar: Ø16mm-310mm
Forging 4140 steel bar: Ø250mm-1000mm
Cold drawn 4140 steel bar:Ø12-100mm
Q&T 4140 steel bar:Ø16-310mm
5.HEAT TREATMENT
Annealing
SCM440 alloy steel is annealed at 872°C (1600°F) followed by slowly cooling in the furnace.
Tempering
SCM4400 alloy steel can be tempered at 205 to 649°C (400 to 1200°F) depending upon the desired hardness level. The hardness of the steel can be increased if it has lower tempering temperature. For example, tensile strength of 225 ksi cab be achieved by tempering at 316°C (600°F), and a tensile strength of 130 ksi can be achieved by tempering at 538°C (1000°F).
Hardening
SCM440 alloy steel can be hardened by cold working, or heating and quenching.
6.QUALITY CONTROL:
1.Processing Line:
Iron - hot metal pretreatment - Converter - Refining --VD / RH- - Continuous Casting - Hot Rolling (KOCKS) - heat --UT Check - Processing and Distribution Center
Electric Furnace - Refining --VD / RH- - Continuous Casting - Hot Rolling (KOCKS) - heat --UT Check - Processing and Distribution Center
2.Gas content level:O2 - <20 ppm H2 - <2 ppm N2- <100 ppm
3.Grain Sizes:5-8
4. non-metallic inclusions contorlling level
A | B | C | D | |
MAX | MAX | MAX | MAX | |
Thin | 2 | 2 | 2 | 2 |
Thick | 1 | 1 | 1 | 1 |